Table of Contents
TPU is the filament that makes people nervous - and for good reason. It’s rubbery, springy, and absolutely does not behave like PLA. Feed it through the wrong printer setup and you’ll end up with a bird’s nest of spaghetti filament jammed in your extruder. But get the setup right and TPU opens up a whole category of prints that no rigid filament can touch.
This guide covers everything you need to print TPU successfully: what it is, what it’s good for, what hardware you need, the right settings, and how to fix the most common problems.
What Is TPU?
TPU stands for Thermoplastic Polyurethane. It’s a flexible, rubber-like filament that belongs to a broader category called elastomers. Unlike PLA or PETG, TPU can be stretched, compressed, and bent without cracking - and it springs back to its original shape.
That flexibility makes it ideal for a wide range of functional prints:
- Phone cases and tablet bumpers - absorbs impact without shattering
- Drone frame bumpers and motor mounts - protects against crash damage
- Gaskets and seals - flexible enough to compress and form a real seal
- RC car tires - grippy, durable, and customizable tread patterns
- Cable strain reliefs - protects cords where they meet connectors
- Shoe insoles and orthotics - custom fit, real cushioning
- Grips and handles - soft-touch finish on rigid assemblies
- Watch bands and wearables - skin-safe and comfortable
If your project needs to flex, grip, seal, or absorb impact, TPU is the material to reach for.
Understanding Shore Hardness
Not all TPU is the same. The key spec to understand is Shore A hardness, which measures how resistant a material is to permanent indentation. Lower numbers are softer and more flexible; higher numbers are firmer.
| Shore Rating | Feel | Best For |
|---|---|---|
| 85A | Very soft, almost squishy | Gaskets, seals, soft grips |
| 87A | Soft with good stretch | Wearables, phone cases |
| 90A | Medium flex | Bumpers, straps |
| 95A | Firm, slight flex | Functional parts, tires |
| 98A | Nearly rigid | Structural parts needing minor flex |
95A is the most common and the easiest to print. It has just enough flex to be useful but enough firmness that it feeds through extruders without too much trouble. If you’re new to TPU, start with 95A before experimenting with softer grades.
Softer materials (85A–87A) are more functional for certain applications but significantly harder to print because they compress easily inside the extruder pathway.
Printer Requirements: Direct Drive vs. Bowden
This is the most important hardware consideration for TPU.
Direct Drive: The Right Tool for the Job
A direct drive extruder sits directly on the print head, so the distance between the drive gear and the nozzle is just a few millimeters. With TPU, that short distance is critical. The filament has almost no room to buckle or coil before it enters the hot end.
Printers with direct drive setups - like the Bambu Lab series, Prusa MK4, Ender 3 with a direct drive upgrade, or any Voron build - handle TPU well right out of the box.
Bowden: It Can Work, But Expect More Effort
A Bowden extruder sits remotely (usually on the frame) and feeds filament through a long PTFE tube to the hot end. That tube can be 300–500mm long. When you try to push flexible TPU through that distance, it compresses and coils inside the tube instead of extruding cleanly.
Printing TPU on a Bowden printer isn’t impossible, but it requires:
- Slowing down significantly (20mm/s or less)
- Using 95A or firmer TPU only - avoid soft grades
- Keeping retraction very low or disabled entirely
- Making sure the PTFE tube fits tightly with no gaps at connections
If you’re on a Bowden printer and printing TPU regularly, a direct drive upgrade is worth every dollar.
Recommended Print Settings
These are solid starting points. Dial them in based on your specific printer and filament brand.
Print Temperature: 220–240°C Most TPU brands print well at 230°C. Go higher if you see under-extrusion; go lower if you see stringing or blobbing. Always check the manufacturer’s recommended range - some specialty TPUs run cooler.
Bed Temperature: 30–60°C TPU sticks well at moderate temps. A PEI spring steel sheet at 45–50°C is ideal. If you’re printing on glass, 55–60°C with a light glue stick application works reliably.
Print Speed: 20–40mm/s Speed is the single biggest lever when printing TPU. Slow down. Seriously. 25–30mm/s is a safe target for most setups. Going faster causes under-extrusion and filament grinding because TPU can’t be pushed through fast - it just compresses.
Retraction: 0–2mm This surprises most people. TPU needs very little retraction, and on direct drive setups, you may get better results with retraction disabled entirely. Too much retraction causes the flexible filament to stretch and then snap back erratically, leading to inconsistent extrusion and jams.
Flow Rate: 100–105% TPU is slightly compressible, so bumping flow up a few percent can help fill gaps and improve layer adhesion. Dial it in with a test cube.
Cooling: 50–100% part cooling Good cooling helps TPU maintain its shape and speeds up bridging. Run your part cooling fan at full speed after the first few layers.
Layer Height: 0.2–0.3mm Standard layer heights work fine. You can go thicker (0.3mm) for functional prints where surface detail matters less - it speeds things up and improves layer bonding.
Common Problems and How to Fix Them
Stringing
TPU strings more than most filaments because it oozes easily at temperature. Fix it by lowering temperature 5°C at a time, reducing travel speed, and enabling combing mode in your slicer to keep the nozzle over the print during travel moves.
Under-Extrusion
Usually caused by printing too fast. Drop your speed to 25mm/s and see if it improves. Also check that the filament path from spool to extruder is smooth with no sharp bends - TPU will kink and jam if it’s fighting resistance on the way in.
Grinding/Stripping at the Extruder
The extruder gear is chewing through the filament instead of pushing it. This means either the idler tension is too high or the print speed is too fast. Back off the idler tension slightly and slow down.
Bed Adhesion Issues
TPU can be finicky on bare glass. Use a PEI build plate, or apply a thin layer of glue stick to glass. Make sure your first layer is slightly squished - a bit more than you’d use for PLA. If the print pops off mid-print, increase bed temperature by 5°C increments.
Jams in Bowden Tubes
If you’re on a Bowden printer and getting jams, the filament is likely coiling inside the tube. Use only 95A or harder TPU, drop speed to 20mm/s, and make sure there are no gaps between the Bowden tube and the nozzle.
Best TPU Brands to Try
Polymaker PolyFlex TPU95 - Widely available, easy to print, good consistency. A reliable starting point for beginners.
Overture TPU - Budget-friendly and works well for most applications. Available in a wide range of colors.
Sainsmart Flexible TPU - Good value, prints reliably at 95A, popular for functional parts and RC tires.
NinjaTek Cheetah - Premium option with excellent quality control. Slightly firmer than standard 95A. Great for production parts.
NinjaTek Armadillo - Harder (75D, which is between standard flex and rigid), designed for high-wear applications like wheels and abrasion-resistant parts.
For soft, specialty applications, Recreus Filaflex (82A and 70A) is excellent but requires a dialed-in direct drive setup.
FAQ
Can I print TPU on an Ender 3? Yes, but the stock Ender 3 has a Bowden setup, which makes TPU challenging. Many users upgrade to a direct drive extruder (like the Sprite or a BMG-based kit) first. With a stock Bowden Ender 3, use only 95A TPU, print at 20mm/s, and minimize retraction.
Do I need a hardened nozzle for TPU? No. TPU is not abrasive, so a standard brass nozzle is fine. Hardened steel nozzles are only needed for abrasive filaments like carbon fiber or glow-in-the-dark PLA.
Why does my TPU look rough or bubbly on the surface? This is usually moisture absorption. TPU is hygroscopic and absorbs humidity from the air. Dry your filament at 45–50°C for 4–6 hours before printing. If you don’t have a dedicated filament dryer, a food dehydrator works well. Store unused TPU in a sealed bag with desiccant packets.
What slicer settings matter most for TPU? Speed, retraction, and combing mode are the big three. Slow down to 25–30mm/s, cut retraction to 1mm or less, and enable combing (or “avoid crossing perimeters”) to reduce travel moves over open air. These three changes alone will solve most TPU printing problems.
TPU rewards patience. The first spool you run through will likely involve some dialing in - a jam here, some stringing there. Once your settings are locked, it prints reliably and opens up functional applications that no other filament can match. Start with 95A, slow down, and give it the time it needs.
Sponsored
Ready to Print?
Browse our guides for more tips on getting the best results from your printer.
Browse All GuidesReady to Print?
Browse our guides for more tips, reviews, and step-by-step tutorials to get the most out of your 3D printer.